Suspensoid of HZSM-5 or HY zeolites mixed with a self-made ceramic-like binder was coated on the inner wall of a tubular reactor by gas-aided fluid displacement technology. The coated zeolites were characterized by means of X-ray diffraction (XRD), Fourier transform infrared spectroscopy (FT-IR) and scanning electron microscopy (SEM). The coating thickness is 10–20 ?m and the particle size of the zeolites is in the range of 1–5 ?m. In the coated reactor, cracking of endothermic fuels including n-dodecane and aviation fuel RP-3 was carried out separately under supercritical conditions at 600°C and 625°C to investigate their heat sinks and conversion of catalytic reactions. For the reaction catalyzed by HY(25% mass fraction) coating, the heat sink capacity of n-dodecane are 815.7 and 901.9 kJ/kg higher than that of the bare tube at 600°C and at 625°C, respectively. Conversion of n-dodecane also increases from 42% to 60% at 600°C and from 66% to 80% at 625°C. The coated zeolite can significantly inhibit the carbon deposition during supercritical cracking reactions.
{{custom_sec.title}}
{{custom_sec.title}}
{{custom_sec.content}}
This is a preview of subscription content, contact
us for subscripton.
References
1. Edwards T Liquidfuels and propellants for aerospace propulsion 1903–2003Journal of Propulsion and Power 2003 19(6)10891107
2. Edwards T Systemdrivers for high heat sink fuelsACS Divisionof Petroleun Chemistry 2000 45(3)436439
3. Cooper M Shepherd J E Experiments studying thermalcracking, catalytic cracking, and pre-mixed partial oxidation of JP-10In: 39th AIAA/ASME/SAE/ASEE Joint propulsion conferenceand ExhibitHuntsvilleAIAA 2003 4687
4. Williams P T Brindle A J Catalytic pyrolysis of tyres:influence of catalyst temperatureFuel 2002 81(18)24252434. doi:10.1016/S0016‐2361(02)00196‐5
5. Babitz S M Williams B A Miller J T Snurr W O H Kung H H Monomolecular cracking of n-hexane on Y, MOR, and ZSM-5 zeolitesAppl Catal A 1999 179(1–2)7186
6. Huang H Spadaccini L J Sobel D R Fuel-cooled thermal management for advanced aeroenginesJ Eng Gas Turb Power-Transactions ASME 2004 126(2)284293. doi:10.1115/1.1689361
7. Soble D R Spadaccini L J Hydrocarbon fuel cooling technologiesfor advanced propulsionJ Eng Gas Turb Power-TransactionsASME 1997 119(4)344351. doi:10.1115/1.2815581
8. Okuyama K Ogawa A Iida Y Reaction and heat transfer characteristics of catalyst-coatedfins (theoretical analysis of fin with an endothermic reaction)JSME Int J 1999 42(2)255261
9. Peters T A van der Tuin J Houssin C Vorstman M A G Benes N E Vroon Z A E P Holmen A Keurentjes J T F Preparation of zeolite-coated pervaporation membranes forthe integration of reaction and separationCatal Today 2005 104(2-4)288295. doi:10.1016/j.cattod.2005.03.065
10. Thijs A P N ieck E B Jos T F K Zeolite-coated ceramic pervaporation membranes: pervaporation-esterificationcoupling and reactorInd Eng Chem Res 2005 44(25)94909496. doi:10.1021/ie0502279
11. Guo W Supercriticalcracking of n-dodecane and RP-3using coating catalysts. Dissertation for the Master Degree.TianjinTianjinUniversity 2006 120 (in Chinese)