Sintering products molded by injecting ceramic and metal powders

Ping-an Liu , Ling-ke Zeng , Xiu-yan Li

Journal of Central South University ›› 2005, Vol. 12 ›› Issue (3) : 269 -271.

PDF
Journal of Central South University ›› 2005, Vol. 12 ›› Issue (3) : 269 -271. DOI: 10.1007/s11771-005-0142-6
Article

Sintering products molded by injecting ceramic and metal powders

Author information +
History +
PDF

Abstract

The injection molding products with different volume ratios of ZrO2 ceramic powder to 316L stainless steel powder were prepared. Properties and structure of the products were characterized by X-ray diffraction (XRD), scanning electron microscope (SEM) and transmission electron microscope (TEM). The results show that the compressive stress exists in the products and the bend strength reaches 300 MPa. ZrO2 phase and stainless steel phase are uniform in samples. The toughness of ceramic increases with the increasing the content of stainless steel. Through TEM study of the interface, some crystalline orientation relationships are determined.

Keywords

metal ceramic / powder injection molding / toughness / stress

Cite this article

Download citation ▾
Ping-an Liu, Ling-ke Zeng, Xiu-yan Li. Sintering products molded by injecting ceramic and metal powders. Journal of Central South University, 2005, 12(3): 269-271 DOI:10.1007/s11771-005-0142-6

登录浏览全文

4963

注册一个新账户 忘记密码

References

[1]

GermanR M, BoseAInjection Molding of Metals and Ceramics[M], 1997, Princeton, Metal Powder Industries Federation

[2]

GermanR M, CornwallR G. Powder injection molding: 2000 market and industry report[J]. Int J Powder Metall, 2001, 37(1): 40-44

[3]

KrajewskiP E, AllisonJ E, JonesJ W. The influence of matrix microstructure and particle reinforcement on the creep behavior of 2219 alumium[J]. Metall Mater Trans A, 1993, 24A(12): 2731-2741

[4]

ChawlaN, HabelU, ShenY L, et al.. The effect of matrix microstructure on the tensile and fatigue behavior of SiC particle reinforced 2080 Al matrix[J]. Metall Mater Trans A, 2000, 31A(2): 531-540

[5]

ChawlaN, AndresdC, JonesJ W, et al.. Effect of SiC volume fraction and particle size on the fatigue resistance of a 2080Al/SiCp composite[J]. Metall Mater Trans A, 1998, 29A(11): 2843-2854

[6]

WangPan-xinPowder Metallurgy [M], 1997, Beijing, Metallurgical Industry Press(in Chinese)

[7]

ZhouYuCeramic Materials [M], 1996, Harbin, Harbin Institute of Technology Press(in Chinese)

[8]

JungY G, PaikU, ChoiS C. Influence of the particle size and phase type of zirconia on the fabrication residual stress of zirconia/stainless-steel 304 functionally gradient material[J]. J Mater Sci, 1999, 34(21): 5407-5416

[9]

LiuYue-hui, LiuPing-anTheory and Application of X-ray Diffraction [M], 2003, Beijing, Chemical Industry Press(in Chinese)