Wear of multifaceted perishable carbide inserts in turning of experimental steel 75ХГСФ

R. B Volkov

Izvestiya MGTU MAMI ›› 2014, Vol. 8 ›› Issue (1-2) : 69 -73.

PDF
Izvestiya MGTU MAMI ›› 2014, Vol. 8 ›› Issue (1-2) : 69 -73. DOI: 10.17816/2074-0530-67731
Articles
research-article

Wear of multifaceted perishable carbide inserts in turning of experimental steel 75ХГСФ

Author information +
History +
PDF

Abstract

The author considers the nature of wear and tear of multifaceted perishable carbide inserts in turning of experimental high-carbon alloy steel 75ХГСФ. Recommendations on choosing the form of inserts, angles of cutting part and types of wear-resistant coatings for flank and face surfaces are given.

Keywords

steel / wear pattern / face surface / flank surface

Cite this article

Download citation ▾
R. B Volkov. Wear of multifaceted perishable carbide inserts in turning of experimental steel 75ХГСФ. Izvestiya MGTU MAMI, 2014, 8(1-2): 69-73 DOI:10.17816/2074-0530-67731

登录浏览全文

4963

注册一个新账户 忘记密码

References

[1]

Режимы резания для токарных и сверлильно-фрезерно-расточных станков. Справочник/ Гузеев В.И., Батуев В.А., Сурков И.В.: М. Машиностроение, 2007 г., 366 с.

[2]

Особенности точения экспериментальной стали 75ХГФС/ Черепахин А.А., Волков Р.Б.: М., Проблемы черной металлургии и материаловедения № 1,.2013 г. - с. 79-83.

[3]

Исследование обрабатываемости стали 75ХГФС/ Р.Б. Волков, А.В, Голобоков, В.А. Кузнецов, А.А. Черепахин: Известия МГТУ «МАМИ», 2012, т. 2, № 2 (14) - с. 51-55.

RIGHTS & PERMISSIONS

Volkov R.B.

AI Summary AI Mindmap
PDF

116

Accesses

0

Citation

Detail

Sections
Recommended

AI思维导图

/