Abstract

A simple method to fabricate one-dimensional (1-D) and two-dimensional (2-D) ordered micro- and nano-scale patterns is developed based on the original masters from optical discs, using nanoimprint technology and soft stamps. Polydimethylsiloxane (PDMS) was used to replicate the negative image of the 1-D grating pattern on the masters of CD-R, DVD-R and BD-R optical discs, respectively, and then the 1-D pattern on one of the PDMS stamps was transferred to a blank polycarbonate (PC) substrate by nanoimprint. The 2-D ordered patterns were fabricated by the second imprinting using another PDMS stamp. Different 2-D periodic patterns were obtained depending on the PDMS stamps and the angle between the two times of imprints. This method may provide a way for the fabrication of complex 2-D patterns using simple 1-D masters.

Cite this article

Download citation ▾
Hui-jing Guo, Xiao-liang Zhang, Xiao-chun Li. Fabrication of ordered micro- and nano-scale patterns based on optical discs and nanoimprint. Optoelectronics Letters, 2016, 12(4): 241-244 DOI:10.1007/s11801-016-6097-z

登录浏览全文

4963

注册一个新账户 忘记密码

References

[1]

Chen J. H., Li Y. Y., Huang K., Wang P. X., He L. L., Carter K. R., Nugen S. R.. ACS Applied Materials & Interfaces. 2015, 7: 22106

[2]

Zhang Y., Yao W. J., Yu H.. Optoelectronics Letters. 2015, 11: 116

[3]

van de Groep J., Spinelli P., Polman A.. Nano Letters. 2015, 15: 4223

[4]

Chou S. Y., Krauss P. R., Renstrom P. J.. Applied Physic Letters. 1995, 67: 3114

[5]

Xuan M. D., Dai L. G., Jia H. Q., Chen H.. Optoelectronics Letters. 2014, 10: 0051

[6]

Dong Q., Xia Y. N., Whitesides G. M.. Nature Protocols. 2010, 5: 491

[7]

Dou X., Phillips B. M., Chung P. Y., Jiang P.. Optics Letters. 2012, 37: 3681

[8]

Dou X., Chung P. Y., Jiang P., Dai J. L.. Applied Physics Letters. 2012, 100: 041116

[9]

Hazarika P., Chowdhury D., Chattopadhyay A.. Lab on a Chip. 2003, 3: 128

[10]

Bhandaru N., Roy S., Harikrishnan G., Mukherjee R.. ACS Macro Letters. 2013, 2: 195

[11]

Leordean C., Gabudean A. M., Canpean V., Astilean S.. Analyst. 2013, 138: 4975

[12]

Goela P., Kumara S., Kapoorb R., Singh J. P.. Applied Surface Science. 2015, 356: 102

[13]

Smith A. J., Wang C., Guo D. N., Sun C., Xia J. X.. Nature Communications. 2014, 5: 5517

[14]

Liu Y. S., Zhang P., Deng Y. B., Hao P., Fan J. H., Chi M. B., Wu Y. H.. Journal of Micromechanics and Microengineering. 2014, 24: 095028

[15]

Lee B. K., Lee B. Y.. Journal of Mechanical Science and Technology. 2015, 29: 5063

PDF

166

Accesses

0

Citation

Detail

Sections
Recommended

/