Effect of complex modification of Al-5Ti and Al-3P on hypereutectic Al-18Si alloys
Jian-hua Wang , Wei Yang , Hao Tu , Ya Liu , Hao-ping Peng , Xu-ping Su
Journal of Central South University ›› 2019, Vol. 26 ›› Issue (10) : 2651 -2660.
Effect of complex modification of Al-5Ti and Al-3P on hypereutectic Al-18Si alloys
The solidification microstructure, fracture morphologies, and mechanical properties of an Al-18Si alloy and alloys modified with Al-5Ti and Al-3P master alloys were investigated using an optical microscope, scanning electron microscope, and an electronic universal testing machine. The results show that additions of Al-5Ti and Al-3P have significant effects on the size and area fraction of the primary Si and the mechanical properties of the Al-18Si alloy. Compared to the Al-18Si alloy modified with 0.6 wt% Al-5Ti at 850 °C, when the Al-18Si alloy was modified with 0.3 wt% Al-5Ti and 0.5 wt% Al-3P at the same temperature, the average size of the primary Si decreased from 39 to 14 μm and the area fraction increased from 9.5% to 11.6%. The biggest influencing factor on the tensile strength and elongation of the Al-18Si alloy is the addition of Al-3P, followed by the modification temperature and the addition of Al-5Ti. At a modification temperature of 850 °C, the tensile strength and elongation of the Al-18Si alloy modified with 0.3 wt% Al-5Ti+0.5 wt% Al-3P increased by 19.6% and 88.6%, respectively compared to that of the Al-18Si alloy modified with 0.6 wt% Al-5Ti.
hypereutectic Al-Si alloy / modification / solidification structure / mechanical properties
| [1] |
|
| [2] |
|
| [3] |
|
| [4] |
|
| [5] |
|
| [6] |
|
| [7] |
|
| [8] |
|
| [9] |
|
| [10] |
|
| [11] |
|
| [12] |
|
| [13] |
|
| [14] |
|
| [15] |
|
| [16] |
|
| [17] |
|
| [18] |
|
| [19] |
|
| [20] |
|
| [21] |
|
| [22] |
|
| [23] |
|
| [24] |
|
| [25] |
|
| [26] |
|
/
| 〈 |
|
〉 |