Thermal behaviors of deactivation catalysts for synthesizing 2, 3, 5-trimethylhydroquinone
Dong Qian , Ai-hua Shi , Qi-yuan Chen , Zhi-jian Liu
Journal of Central South University ›› 2005, Vol. 12 ›› Issue (Suppl 1) : 65 -67.
Thermal behaviors of deactivation catalysts for synthesizing 2, 3, 5-trimethylhydroquinone
The thermal behaviors of the deposits on supported noble metal catalysts for synthesizing 2, 3, 5-trimethylhydroquinone by DSC were studied. The results show that the supported Pd catalysts have two exothermic peaks at around 312 °C and 435 °C in the DSC thermograms, respectively, while the supported Pt catalysts have one exothermic peak at approximately 345 °C. Therefore, it is supposed that the adsorptive states of deposits on supported Pt catalysts and supported Pd catalysts are different, which may be one reason leading to the stability difference between supported Pt catalysts and supported Pd catalysts.
deposit / supported Pd catalysts / supported Pt catalysts / DSC
| [1] |
|
| [2] |
|
| [3] |
Michelet D, Razoutz M. Process for the Preparation of Trimethyl-para-benzaquinone[P]. US 3927045. 1975 - 12 - 16. |
| [4] |
Kawaguchi T, Nishida T, Ohmura Y, et al. Process for Preparing of 2, 3, 5-trimethylhydroquinone[P]. US 3842130. 1974 - 10 - 15. |
| [5] |
|
| [6] |
YANG Li-yi, ZHANG Mou-kun, QIAN Dong, et al. Studies on the continuous process for synthesizing 2, 3, 5-trimethylhydroquinone with Pt/Al2O3 catalyst [J]. Speciality Petrochemicals, 1998(5): 27–29. (in Chinese) |
| [7] |
|
| [8] |
|
| [9] |
|
| [10] |
|
| [11] |
Yui T, Ito A. Process for Preparation of 2, 3, 5-trimethylhydroquinone[P]. US 4769500. 1988 - 09 - 06. |
| [12] |
|
/
| 〈 |
|
〉 |