PDF
Abstract
More research is needed to assess whether all-ceramic crowns accelerate the rate of tooth wear in molars and premolars, conclude two dentists in Germany who systematically reviewed the dental literature. Rim Hmaidouch and Paul Weigl from the Johann Wolfgang Goethe University in Frankfurt, searched for published studies that investigated whether a causal relationship exists between the insertions of ceramic crowns and increased wear in the posterior dental region. They found only five studies that examined the issue, including three that evaluated tooth wear in the exact same patient population. From the three independent pools of study subjects, the authors determined that some ceramic materials are wear-friendly. However, the published studies suffered from many design flaws, so they believe that additional, more rigorous clinical trials are still warranted.
Keywords
all-ceramic
/
crowns
/
tooth wear
Cite this article
Download citation ▾
Rim Hmaidouch, Paul Weigl.
Tooth wear against ceramic crowns in posterior region: a systematic literature review.
International Journal of Oral Science, 2013, 5(4): 183-190 DOI:10.1038/ijos.2013.73
| [1] |
Wiley MG. Effects of porcelain on occluding surfaces of restored teeth. J Prosthet Dent, 1989, 61(2): 133-137.
|
| [2] |
Sulong MZ, Aziz RA. Wear of materials used in dentistry: a review of the literature. J Prosthet Dent, 1990, 63(3): 342-349.
|
| [3] |
Bani D, Bani T, Bergamini M. Morphologic and biochemical changes of the masseter muscles induced by occlusal wear: studies in a rat model. J Dent Res, 1999, 78(11): 1735-1744.
|
| [4] |
Oh WS, Delong R, Anusavice KJ. Factors affecting enamel and ceramic wear: a literature review. J Prosthet Dent, 2002, 87(4): 451-459.
|
| [5] |
Ohlmann B, Trame JP, Dreyhaupt J. Wear of posterior metal-free polymer crowns after 2 years. J Oral Rehabil, 2008, 35(10): 782-788.
|
| [6] |
Smith BG, Bartlett DW, Robb ND. The prevalence, etiology and management of tooth wear in the United Kingdom. J Prosthet Dent, 1997, 78(4): 367-372.
|
| [7] |
Xhonga FA. Bruxism and its effect on the teeth. J Oral Rehabil, 1977, 4(1): 65-76.
|
| [8] |
Addy M, Hunter ML. Can tooth brushing damage your health? Effects on oral and dental tissues. Int Dent J, 2003, 53(Suppl 3): 177-186.
|
| [9] |
Absi EG, Addy M, Adams D. Dentine hypersensitivity - the effect of toothbrushing and dietary compounds on dentine in vitro: an SEM study. J Oral Rehabil, 1992, 19: 101-110.
|
| [10] |
Huysmans MC, Chew HP, Ellwood RP. Clinical studies of dental erosion and erosive wear. Caries Res, 2011, 45(Suppl 1): 60-68.
|
| [11] |
Lussi A, Schlueter N, Rakhmatullina E. Dental erosion—an overview with emphasis on chemical and histopathological aspects. Caries Res, 2011, 45(Suppl 1): 2-12.
|
| [12] |
Attin T, Buchalla W, Gollner M. Use of variable remineralization periods to improve the abrasion resistance of previously eroded enamel. Caries Res, 2000, 34(1): 48-52.
|
| [13] |
Eisenburger M, Addy M, Hughes JA. Effect of time on the remineralisation of enamel by synthetic saliva after citric acid erosion. Caries Res, 2001, 35(3): 211-215.
|
| [14] |
Ganss C, Klimek J, Schaffer U. Effectiveness of two fluoridation measures on erosion progression in human enamel and dentine in vitro. Caries Res, 2001, 35(5): 325-330.
|
| [15] |
Al-Omiri MK, Harb R, Abu Hammad OA. Quantification of tooth wear: conventional vs new method using toolmakers microscope and a three-dimensional measuring technique. J Dent, 2010, 38(7): 560-568.
|
| [16] |
Carlsson GE, Johansson A, Lundqvist S. Occlusal wear. A follow-up study of 18 subjects with extensively worn dentitions. Acta Odontol Scand, 1985, 43(2): 83-90.
|
| [17] |
Chadwick RG, McCabe JF, Walls AW. Comparison of a novel photogrammetric technique and modified USPHS criteria to monitor the wear of restorations. J Dent, 1991, 19(1): 39-45.
|
| [18] |
Fares J, Shirodaria S, Chiu K. A new index of tooth wear. Reproducibility and application to a sample of 18- to 30-year-old university students. Caries Res, 2009, 43(2): 119-125.
|
| [19] |
Hugoson A, Bergendal T, Ekfeldt A. Prevalence and severity of incisal and occlusal tooth wear in an adult Swedish population. Acta Odontol Scand, 1988, 46(5): 255-265.
|
| [20] |
Oilo G, Dahl BL, Hatle G. An index for evaluating wear of teeth. Acta Odontol Scand, 1987, 45(5): 361-365.
|
| [21] |
Taylor DF, Bayne SC, Sturdevant JR. Correlation of M–L, Leinfelder, and USPHS clinical evaluation techniques for wear. Dent Mater, 1990, 6(3): 151-153.
|
| [22] |
Etman MK, Woolford M, Dunne S. Quantitative measurement of tooth and ceramic wear: in vivo study. Int J Prosthodont, 2008, 21(3): 245-252.
|
| [23] |
Lambrechts P, Braem M, Vuylsteke-Wauters M. Quantitative in vivo wear of human enamel. J Dent Res, 1989, 68(12): 1752-1754.
|
| [24] |
Peters MC, Delong R, Pintado MR. Comparison of two measurement techniques for clinical wear. J Dent, 1999, 27(7): 479-485.
|
| [25] |
Suputtamongkol K, Anusavice KJ, Suchatlampong C. Clinical performance and wear characteristics of veneered lithia-disilicate-based ceramic crowns. Dent Mater, 2008, 24(5): 667-673.
|
| [26] |
Teaford MF, Tylenda CA. A new approach to the study of tooth wear. J Dent Res, 1991, 70(3): 204-207.
|
| [27] |
Willems G, Lambrechts P, Lesaffre E. Three-year follow-up of five posterior composites: SEM study of differential wear. J Dent, 1993, 21(2): 79-86.
|
| [28] |
DeLong R, Sasik C, Pintado MR. The wear of enamel when opposed by ceramic systems. Dent Mater, 1989, 5(4): 266-271.
|
| [29] |
Albashaireh ZS, Ghazal M, Kern M. Two-body wear of different ceramic materials opposed to zirconia ceramic. J Prosthet Dent, 2010, 104(2): 105-113.
|
| [30] |
Mehl A, Gloger W, Kunzelmann KH. A new optical 3-D device for the detection of wear. J Dent Res, 1997, 76(11): 1799-1807.
|
| [31] |
Alarcon JV, Engelmeier RL, Powers JM. Wear testing of composite, gold, porcelain, and enamel opposing a removable cobalt–chromium partial denture alloy. J Prosthodont, 2009, 18(5): 421-426.
|
| [32] |
Delong R, Pintado MR, Douglas WH. The wear of enamel opposing shaded ceramic restorative materials: an in vitro study. J Prosthet Dent, 1992, 68(1): 42-48.
|
| [33] |
Elmaria A, Goldstein G, Vijayaraghavan T. An evaluation of wear when enamel is opposed by various ceramic materials and gold. J Prosthet Dent, 2006, 96(5): 345-353.
|
| [34] |
Hudson JD, Goldstein GR, Georgescu M. Enamel wear caused by three different restorative materials. J Prosthet Dent, 1995, 74(6): 647-654.
|
| [35] |
Joshi N, Patil NP, Patil SB. The abrasive effect of a porcelain and a nickel–chromium alloy on the wear of human enamel and the influence of a carbonated beverage on the rate of wear. J Prosthodont, 2010, 19(3): 212-217.
|
| [36] |
Magne P, Oh WS, Pintado MR. Wear of enamel and veneering ceramics after laboratory and chairside finishing procedures. J Prosthet Dent, 1999, 82(6): 669-679.
|
| [37] |
Metzler KT, Woody RD, Miller AW 3rd. In vitro investigation of the wear of human enamel by dental porcelain. J Prosthet Dent, 1999, 81(3): 356-364.
|
| [38] |
O’Kray HP, O’Brien WJ. In vitro human enamel wear by a hydrated high-alkali porcelain. Quintessence Int, 2005, 36(8): 617-622.
|
| [39] |
Palmer DS, Barco MT, Pelleu GB Jr. Wear of human enamel against a commercial castable ceramic restorative material. J Prosthet Dent, 1991, 65(2): 192-195.
|
| [40] |
Pintado MR, Anderson GC, DeLong R. Variation in tooth wear in young adults over a two-year period. J Prosthet Dent, 1997, 77(3): 313-320.
|
| [41] |
Yu H, Wegehaupt FJ, Wiegand A. Erosion and abrasion of tooth-colored restorative materials and human enamel. J Dent, 2009, 37(12): 913-922.
|
| [42] |
Esquivel-Upshaw JF, Young H, Jones J. In vivo wear of enamel by a lithia disilicate-based core ceramic used for posterior fixed partial dentures: first-year results. Int J Prosthodont, 2006, 19(4): 391-396.
|
| [43] |
DeLong R. Intra-oral restorative materials wear: rethinking the current approaches: how to measure wear. Dent Mater, 2006, 22(8): 702-711.
|
| [44] |
Kobayashi K, Shimoda S, Nakagawa Y. Accuracy in measurement of distance using limited cone-beam computerized tomography. Int J Oral Maxillofac Implants, 2004, 19(2): 228-231.
|
| [45] |
Sirona Dental Systems, Inc. Electronical material cerec omnicam and cerec bluecam. The first choice in every case. Sirona product information. Available at http://www.sirona.com/de/aktuelles/kampagnen/die-neue-cerec-omnicam/ (accessed 31 October 2012).
|
| [46] |
al-Hiyasat AS, Saunders WP, Sharkey SW. Investigation of human enamel wear against four dental ceramics and gold. J Dent, 1998, 26(5/6): 487-495.
|
| [47] |
al-Hiyasat AS, Saunders WP, Smith GM. Three-body wear associated with three ceramics and enamel. J Prosthet Dent, 1999, 82(4): 476-481.
|
| [48] |
Clelland NL, Agarwala V, Knobloch LA. Wear of enamel opposing low-fusing and conventional ceramic restorative materials. J Prosthodont, 2001, 10(1): 8-15.
|
| [49] |
Hacker CH, Wagner WC, Razzoog ME. An in vitro investigation of the wear of enamel on porcelain and gold in saliva. J Prosthet Dent, 1996, 75(1): 14-17.
|
| [50] |
Rosentritt M, Hmaidouch R, Behr M. Fracture resistance of zirconia FPDs with adhesive bonding versus conventional cementation. Int J Prosthodont, 2011, 24(2): 168-171.
|
| [51] |
Heintze SD. How to qualify and validate wear simulation devices and methods. Dent Mater, 2006, 22(8): 712-734.
|
| [52] |
Cattell MJ, Clarke RL, Lynch EJ. The biaxial flexural strength and reliability of four dental ceramics—Part II. J Dent, 1997, 25(5): 409-414.
|
| [53] |
Zarone F, Russo S, Sorrentino R. From porcelain-fused-to-metal to zirconia: clinical and experimental considerations. Dent Mater, 2011, 27(1): 83-96.
|
| [54] |
Scherrer SS, de Rijk WG, Belser UC. Fracture resistance of human enamel and three all-ceramic crown systems on extracted teeth. Int J Prosthodont, 1996, 9(6): 580-585.
|
| [55] |
Aboushelib MN, de Jager N, Kleverlaan CJ. Microtensile bond strength of different components of core veneered all-ceramic restorations. Dent Mater, 2005, 21(10): 984-991.
|
| [56] |
Sundh A, Sjogren G. Fracture resistance of all-ceramic zirconia bridges with differing phase stabilizers and quality of sintering. Dent Mater, 2006, 22(8): 778-784.
|
| [57] |
Raigrodski AJ, Chiche GJ, Potiket N. The efficacy of posterior three-unit zirconium-oxide-based ceramic fixed partial dental prostheses: a prospective clinical pilot study. J Prosthet Dent, 2006, 96(4): 237-244.
|
| [58] |
Esquivel-Upshaw JF, Anusavice KJ, Young H. Clinical performance of a lithia disilicate-based core ceramic for three-unit posterior FPDs. Int J Prosthodont, 2004, 17(4): 469-475.
|
| [59] |
Wolfart S, Bohlsen F, Wegner SM. A preliminary prospective evaluation of all-ceramic crown-retained and inlay-retained fixed partial dentures. Int J Prosthodont, 2005, 18(6): 497-505.
|
| [60] |
Fisher RM, Moore BK, Swartz ML. The effects of enamel wear on the metal-porcelain interface. J Prosthet Dent, 1983, 50(5): 627-631.
|
| [61] |
Dahl BL, Oilo G. In vivo wear ranking of some restorative materials. Quintessence Int, 1994, 25(8): 561-565.
|
| [62] |
Seghi RR, Rosenstiel SF, Bauer P. Abrasion of human enamel by different dental ceramics in vitro. J Dent Res, 1991, 70(3): 221-225.
|
| [63] |
Aboushelib MN, de Jager N, Kleverlaan CJ. Effect of loading method on the fracture mechanics of two layered all-ceramic restorative systems. Dent Mater, 2007, 23(8): 952-959.
|
| [64] |
Guazzato M, Albakry M, Ringer SP. Strength, fracture toughness and microstructure of a selection of all-ceramic materials. Part II. Zirconia-based dental ceramics. Dent Mater, 2004, 20(5): 449-456.
|
| [65] |
Jung YS, Lee JW, Choi YJ. A study on the in-vitro wear of the natural tooth structure by opposing zirconia or dental porcelain. J Adv Prosthodont, 2010, 2(3): 111-115.
|
| [66] |
Rosentritt M, Preis V, Behr M. Two-body wear of dental porcelain and substructure oxide ceramics. Clin Oral Investig, 2012, 16(3): 935-943.
|
| [67] |
Koran A, Craig RG, Tillitson EW. Coefficient of friction of prosthetic tooth materials. J Prosthet Dent, 1972, 27(3): 269-274.
|
| [68] |
Cheung KC, Darvell BW. Sintering of dental porcelain: effect of time and temperature on appearance and porosity. Dent Mater, 2002, 18(2): 163-173.
|
| [69] |
DeLong R, Douglas WH, Sakaguchi RL. The wear of dental porcelain in an artificial mouth. Dent Mater, 1986, 2(5): 214-219.
|
| [70] |
Kelly JR, Campbell SD, Bowen HK. Fracture-surface analysis of dental ceramics. J Prosthet Dent, 1989, 62(5): 536-541.
|
| [71] |
Rasmussen ST, Ngaji-Okumu W, Boenke K. Optimum particle size distribution for reduced sintering shrinkage of a dental porcelain. Dent Mater, 1997, 13(1): 43-50.
|
| [72] |
Anusavice KJ, Lee RB. Effect of firing temperature and water exposure on crack propagation in unglazed porcelain. J Dent Res, 1989, 68(6): 1075-1081.
|
| [73] |
Piddock V. Effect of alumina concentration on the thermal diffusivity of dental porcelain. J Dent, 1989, 17(6): 290-294.
|
| [74] |
Evans DB, Barghi N, Malloy CM. The influence of condensation method on porosity and shade of body porcelain. J Prosthet Dent, 1990, 63(4): 380-389.
|
| [75] |
Centre AAC . Zirluna (translucent) data sheet. Amberg: Centre AAC, 2010.
|
| [76] |
Brewer JD, Garlapo DA, Chipps EA. Clinical discrimination between autoglazed and polished porcelain surfaces. J Prosthet Dent, 1990, 64(6): 631-634.
|
| [77] |
Jagger DC, Harrison A. An in vitro investigation into the wear effects of unglazed, glazed, and polished porcelain on human enamel. J Prosthet Dent, 1994, 72(3): 320-323.
|
| [78] |
Campbell SD. Evaluation of surface roughness and polishing techniques for new ceramic materials. J Prosthet Dent, 1989, 61(5): 563-568.
|
| [79] |
Patterson CJ, McLundie AC, Stirrups DR. Efficacy of a porcelain refinishing system in restoring surface finish after grinding with fine and extra-fine diamond burs. J Prosthet Dent, 1992, 68(3): 402-406.
|
| [80] |
Grieve AR, Jeffrey IW, Sharma SJ. An evaluation of three methods of polishing porcelain by comparison of surface topography with the original glaze. Restorative Dent, 1991, 7(2): 34-36.
|
| [81] |
Sulik WD, Plekavich EJ. Surface finishing of dental porcelain. J Prosthet Dent, 1981, 46(2): 217-221.
|
| [82] |
Haywood VB, Heymann HO, Kusy RP. Polishing porcelain veneers: an SEM and specular reflectance analysis. Dent Mater, 1988, 4(3): 116-121.
|
| [83] |
Haywood VB, Heymann HO, Scurria MS. Effects of water, speed, and experimental instrumentation on finishing and polishing porcelain intra-orally. Dent Mater, 1989, 5(3): 185-188.
|
| [84] |
Scurria MS, Powers JM. Surface roughness of two polished ceramic materials. J Prosthet Dent, 1994, 71(2): 174-177.
|
| [85] |
al-Hiyasat AS, Saunders WP, Sharkey SW. The abrasive effect of glazed, unglazed, and polished porcelain on the wear of human enamel, and the influence of carbonated soft drinks on the rate of wear. Int J Prosthodont, 1997, 10(3): 269-282.
|
| [86] |
Jacobi R, Shillingburg HT Jr, Duncanson MG Jr. A comparison of the abrasiveness of six ceramic surfaces and gold. J Prosthet Dent, 1991, 66(3): 303-309.
|
| [87] |
Monasky GE, Taylor DF. Studies on the wear of porcelain, enamel, and gold. J Prosthet Dent, 1971, 25(3): 299-306.
|
| [88] |
Silva NR, Thompson VP, Valverde GB. Comparative reliability analyses of zirconium oxide and lithium disilicate restorations in vitro and in vivo. J Am Dent Assoc, 2011, 142(Suppl 2): 4S-9S.
|
| [89] |
Esquivel-Upshaw JF, Rose WF Jr, Barrett AA. Three years in vivo wear: core-ceramic, veneers, and enamel antagonists. Dent Mater, 2012, 28(6): 615-621.
|
| [90] |
Esquivel-Upshaw J, Rose W, Oliveira E. Randomized, controlled clinical trial of bilayer ceramic and metal-ceramic crown performance. J Prosthodont, 2013, 22(3): 166-173.
|