Microstructure and mechanical properties of friction welded carbon steel (EN24) and nickel-based superalloy (IN718)

V. T. Gaikwad , M. K. Mishra , V. D. Hiwarkar , R. K. P. Singh

International Journal of Minerals, Metallurgy, and Materials ›› 2021, Vol. 28 ›› Issue (1) : 111 -119.

PDF
International Journal of Minerals, Metallurgy, and Materials ›› 2021, Vol. 28 ›› Issue (1) : 111 -119. DOI: 10.1007/s12613-020-2008-1
Article

Microstructure and mechanical properties of friction welded carbon steel (EN24) and nickel-based superalloy (IN718)

Author information +
History +
PDF

Abstract

Continuous-drive rotary friction welding was performed to join cylindrical specimens of carbon steel (EN24) and nickel-based superalloy (IN718), and the microstructures of three distinct weld zones—the weld interface (WI)/thermo-mechanically affected zone (TMAZ), the heat-affected zone (HAZ), and the base metal—were examined. The joint was observed to be free of defects but featured uneven flash formation. Electron backscatter diffraction (EBSD) analysis showed substantial changes in high-angle grain boundaries, low-angle grain boundaries, and twin boundaries in the TMAZ and HAZ. Moreover, significant refinement in grain size (2–5 μm) was observed at the WI/TMAZ with reference to the base metal. The possible causes of these are discussed. The microhardness profile across the welded joint shows variation in hardness. The changes in hardness are ascribed to grain refinement, phase transformation, and the dissolution of strengthening precipitates. The tensile test results reveal that a joint efficiency of 100% can be achieved using this method.

Keywords

friction welding / dissimilar metals / EN24 / IN718 / microstructure / mechanical properties

Cite this article

Download citation ▾
V. T. Gaikwad, M. K. Mishra, V. D. Hiwarkar, R. K. P. Singh. Microstructure and mechanical properties of friction welded carbon steel (EN24) and nickel-based superalloy (IN718). International Journal of Minerals, Metallurgy, and Materials, 2021, 28(1): 111-119 DOI:10.1007/s12613-020-2008-1

登录浏览全文

4963

注册一个新账户 忘记密码

References

[1]

J. Manuf. Sci. Eng., 2019, 141(3)

[2]

Li WY, Vairis A, Preuss M, Ma TJ. Linear and rotary friction welding review. Int. Mater. Rev., 2016, 61(2): 71.

[3]

American Welding Society American National Standard ANSI/AWS C6.1-89 R2009. Recommended Practice for Friction Welding, 1989, Miami, American National Standards Institute

[4]

Donachie MJ, Donachie SJ. Superalloys: A Technical Guide, 2002, 2nd ed, Materials Park, ASM international, 245.

[5]

Lalam SV, Reddy GM, Mohandas T, Kamaraj M, Murty BS. Continuous drive friction welding of Inconel 718 and EN24 dissimilar metal combination. Mater. Sci. Technol., 2009, 25(7): 851.

[6]

Ma H, Qin GL, Geng PH, Li F, Fu BL, Meng XM. Microstructure characterization and properties of carbon steel to stainless steel dissimilar metal joint made by friction welding. Mater. Des., 2015, 86, 587.

[7]

Paventhan R, Lakshminarayanan PR, Balasubramanian V. Fatigue behaviour of friction welded medium carbon steel and austenitic stainless steel dissimilar joints. Mater. Des., 2011, 32(4): 1888.

[8]

Ma H, Qin GL, Geng PH, Li F, Meng XG, Fu BL. Effect of post-weld heat treatment on friction welded joint of carbon steel to stainless steel. J. Mater. Process. Technol., 2016, 227, 24.

[9]

Wanjara P, Gholipour J, Watanabe K, Nezaki K, Tian Y, Brochu M. Linear friction welding of IN718 to Ti6Al4V. Mater. Sci. Forum, 2017, 879, 2072.

[10]

Cheepu M, Che WS. Characterization of microstructure and interface reactions in friction welded bimetallic joints of titanium to 304 stainless steel using nickel interlayer. Trans. Indian Inst. Met., 2019, 72(6): 1597.

[11]

Huang ZW, Li HY, Pruess M, Karadge M, Bowen P, Bray S, Baxter G. Inertia friction welding dissimilar nickel-based superalloys alloy 720LI to IN718. Metall. Mater. Trans. A, 2007, 38(7): 1608.

[12]

Damodaram R, Raman SGS, Rao KP. Microstructure and mechanical properties of friction welded alloy 718. Mater. Sci. Eng. A, 2013, 560, 781.

[13]

Sahin M, Akata HE, Gulmez T. Characterization of mechanical properties in AISI 1040 parts welded by friction welding. Mater. Charact., 2007, 58(10): 1033.

[14]

Anitha P, Majumder MC, Saravanan V, Rajakumar S. Microstructural characterization and mechanical properties of friction-welded IN718 and SS410 dissimilar joint. Metall. Microstruct. Anal., 2018, 87(3): 277.

[15]

Khidhir GI, Baban SA. Efficiency of dissimilar friction welded 1045 medium carbon steel and 316L austenitic stainless steel joints. J. Mater. Res. Technol., 2019, 8(2): 1926.

[16]

Kimur M, Nakashima K, Kusaka M, Kaizu K, Nakatani Y, Takahashi M. Joining phenomena and tensile strength of joint between Ni-based superalloy and heat-resistant steel by friction welding. Int. J. Adv. Manuf. Technol., 2019, 103(1–4): 1297.

[17]

Wang HJ, Ikeuchi K, Aritoshi M, Takahashi M, Ikeda A. Joint strength of Inconel 718 alloy and its improvement by post-weld heat treatment-joint performance and its controlling factors in friction welding of Inconel 718 alloy. Weld. Int., 2009, 23(9): 679.

[18]

Damodaram R, Ganesh Sundara Raman S, Prasad Rao K. Effect of post-weld heat treatments on microstructure and mechanical properties of friction welded alloy 718 joints. Mater. Des., 2014, 53, 954.

[19]

Madhusudhan Reddy G, Venkata Ramana P. Role of nickel as an interlayer in dissimilar metal friction welding of maraging steel to low alloy steel. J. Mater. Process. Technol., 2012, 212(1): 66.

[20]

Woolman J, Mottram RA. The Mechanical and Physical Properties of the British Standard EN steels (B.S. 970–1955): En 21 to En 39, 1966 87.

[21]

Gaikwad VT, Hiwarkar VD, Pawar VP, Singh RKP. Microstructure characterization and evaluation of mechanical properties for friction welded En-24 alloy steel. Materials Science & Technology (MS&T)2018, 2018 822.

[22]

Wang Y, Shao WZ, Zhen L, Zhang XM. Microstructure evolution during dynamic recrystallization of hot deformed superalloy 718. Mater. Sci. Eng. A, 2008, 486(1–2): 321.

[23]

Zheng YX, Wang FN, Li CR, Li YL, Cheng J, Cao RF. Effect of microstructure and precipitates on mechanical properties of Cr-Mo-V alloy steel with different austenitizing temperatures. ISIJ Int., 2018, 58(6): 1126.

[24]

Mishra MK, Rao AG, Balasundar I, Kashyap BP, Prabhu N. On the microstructure evolution in friction stir processed 2507 super duplex stainless steel and its effect on tensile behaviour at ambient and elevated temperatures. Mater. Sci. Eng. A, 2018, 719, 82.

[25]

Jeon J, Mironov S, Sato YS, Kokawa H, Park SCH, Hirano S. Friction stir spot welding of single-crystal austenitic stainless steel. Acta Mater., 2011, 59(20): 7439.

[26]

Patel V, Li WY, Vairis A, Badheka V. Recent development in friction stir processing as a solid - state grain refinement technique: microstructural evolution and property enhancement. Crit. Rev. Solid State Mater. Sci., 2019, 44(5): 378.

[27]

Aktarer SM, Sekban DM, Kucukomeroglu T, Purcek G. Microstructure, mechanical properties and formability of friction stir welded dissimilar materials of IF-steel and 6061 Al alloy. Int. J. Miner. Metall. Mater., 2019, 26(6): 722.

AI Summary AI Mindmap
PDF

175

Accesses

0

Citation

Detail

Sections
Recommended

AI思维导图

/