Soft chemical synthesis and luminescence properties of red long-lasting phosphors Y2O2S:Sm3+
Yan-juan Li , Ming-wen Wang , Lu-dan Zhang , Duo Gao , Shi-xiang Liu
International Journal of Minerals, Metallurgy, and Materials ›› 2013, Vol. 20 ›› Issue (10) : 972 -977.
Soft chemical synthesis and luminescence properties of red long-lasting phosphors Y2O2S:Sm3+
Sm3+-activated Y2O2S red phosphors were prepared by the combustion method and microemulsion method at the first time. X-ray characterization and electron diffraction show that, Y2O2S:Sm3+, Ti4+, Mg2+ samples prepared by these two methods are pure hexagonal crystals in structure with a trivial change due to dopants. Scanning electron microscopy (SEM) results show that the product presents an almond-like sheet in uniform size. Under the excitation of 269 nm ultraviolet light, Y2O2S:Sm3+ samples fabricated by these two methods exhibit three main groups of red emission lines located at 564, 604, and 656 nm, respectively, which are attributed to the transitions of 4G5/2 →6H5/2, 4G5/2 →6H7/2, 4G5/2 →6H9/2, respectively. The samples prepared by microemulsion are seven times higher in fluorescent emission intensity and half time longer in afterglow time than that prepared by combustion.
phosphors / soft chemical synthesis / luminescence / combustion / microemulsion
| [1] |
|
| [2] |
|
| [3] |
|
| [4] |
|
| [5] |
|
| [6] |
|
| [7] |
|
| [8] |
|
| [9] |
|
| [10] |
|
| [11] |
|
| [12] |
|
| [13] |
|
| [14] |
|
| [15] |
|
| [16] |
|
| [17] |
|
| [18] |
|
| [19] |
|
/
| 〈 |
|
〉 |