NaOH-activated slow-release energy material agents for rock preconditioning: Enhanced expansive pressure and a mechanistic framework
Yutong Gui , P. G. Ranjith
International Journal of Minerals, Metallurgy and Materials ›› 2026, Vol. 33 ›› Issue (8) : 2527 -2540.
With the increasing global demand for critical minerals and low-impact subsurface energy systems, efficient and sustainable rock preconditioning methods are urgently needed. Slow-release energy material agents (SREMAs) are promising next-generation materials for enhancing rock permeability, with potential applications in mineral recovery, geothermal stimulation, and underground hydrogen storage. However, their broader adoption has been limited by suboptimal expansive pressure and a lack of mechanistic understanding. This study addresses both challenges by incorporating sodium hydroxide (NaOH) as an inorganic accelerator to enhance the performance and reveal the underlying expansion mechanism. Seven SREMAs formulations with varying NaOH contents were evaluated using the outer pipe method, and three representative samples were characterized using inductively coupled plasma mass spectrometry, scanning electron microscopy, and X-ray diffraction. The results show that NaOH accelerates hydration reactions and increases 24-h expansive pressure by 15.03% to 52.62%, with a peak performance at 0.15wt% NaOH. NaOH addition promoted the formation of calcium hydroxide and ettringite and optimized the microporous structure of calcium silicate hydrate, the latter playing a critical role in transforming internal expansion into effective outward pressure. A novel mechanistic framework linking mineralogical transformations to enhanced macroscopic performance is proposed. This study provides new insights into sustainable rock preconditioning and offers a foundation for optimizing SREMAs for applications in which low-carbon, high-efficiency subsurface engineering is essential.
slow-release energy material agents / thermodynamic equilibrium / mineralogical transformation / expansion mechanism / sustainable subsurface engineering / mineral recovery
| [1] |
O. Vidal, H. Le Boulzec, B. Andrieu, and F. Verzier, Modelling the demand and access of mineral resources in a changing world, Sustainability, 14(2022), No. 1, art. No. 11. |
| [2] |
|
| [3] |
|
| [4] |
G. Calvo, G. Mudd, A. Valero, and A. Valero, Decreasing ore grades in global metallic mining: A theoretical issue or a global reality, Resources, 5(2016), No. 4, art. No. 36. |
| [5] |
|
| [6] |
|
| [7] |
|
| [8] |
|
| [9] |
|
| [10] |
R.V. De Silva, R. Pathegama Gamage, and M.S. Anne Perera, An alternative to conventional rock fragmentation methods using SCDA: A review. Energies, 9(2016), No. 11, art. No. 958. |
| [11] |
|
| [12] |
Z. Zhong, Y.H. Cui, P. Tao, C. Gao, R. Lou, and J. Liu, Quantitative assessment and optimized utilization of soundless cracking demolition agent for fragmentations of basalt fiber–reinforced concrete, J. Mater. Civ. Eng., 37(2025), No. 3, art. No. 04025010. |
| [13] |
|
| [14] |
K. Kim, H. Cho, D. Sohn, and J. Lee, The use of expansive chemical agents for concrete demolition: Example of practical design and application, Constr. Build. Mater., 272(2021), art. No. 121849. |
| [15] |
|
| [16] |
|
| [17] |
|
| [18] |
|
| [19] |
T. Kannangara and P.G. Ranjith, Revolutionizing mineral recovery: The untapped potential of non-explosive expansive agents for eco-friendly mining, Sustain. Mater. Technol., 43(2025), art. No. e01238. |
| [20] |
T. Kannangara, P.G. Ranjith, and V.R.S. De Silva, Eco-friendly rock fracturing: Enhancing SREMA with calcium sulfate for sustainable mineral recovery, Mater. Today Sustain., 31(2025), art. No. 101167. |
| [21] |
|
| [22] |
X.Y. Zhu, C. Zhai, J.Z. Xu, Y. Sun, Y.F. Zheng, and H.X. Xu, Investigation of hydration mechanism of non-explosive expansion material modified with anhydrous calcium chloride, Adv. Powder Technol., 35(2024), No. 5, art. No. 104433. |
| [23] |
X.Y. Zhu, C. Zhai, X. Yu, et al., Effects of anhydrous CaCl2 on flocculation characteristics, rheological properties and blowout inhibition mechanism of non-explosive expansive cement, Constr. Build. Mater., 456(2024), art. No. 139167. |
| [24] |
|
| [25] |
T.J. Huang, K. Zhang, K.G. Kang, and Q. Yuan, The effect of NaOH addition on the physico-chemical phenomena of cement setting acceleration, Constr. Build. Mater., 458(2025), art. No. 139761. |
| [26] |
Z. Zheng, J. Yang, H.R. Fu, et al., The coupling impact of Na-OH and NaNO3 on hydration process, products and Sr2+ adsorption ability of the major phases in Portland cement, Constr. Build Mater., 459(2025), art. No. 139813. |
| [27] |
Z.Q. Zhang, Y. Shao, L. Huang, X.M. Liu, F.H. Han, and P.Y. Yan, A new hydration kinetic model based on boundary nucleation and growth mechanism with time-dependent growth rate: Application to quantitively characterize the influence of alkali on the early hydration of cement, Constr. Build. Mater., 411(2024), art. No. 134616. |
| [28] |
Y.R. Yan, S.Y. Yang, G.D. Miron, et al., Effect of alkali hydroxide on calcium silicate hydrate (C–S–H), Cem. Concr. Res., 151(2022), art. No. 106636. |
| [29] |
|
| [30] |
|
| [31] |
|
| [32] |
|
| [33] |
|
| [34] |
|
| [35] |
|
| [36] |
|
| [37] |
|
| [38] |
|
| [39] |
|
| [40] |
|
| [41] |
|
| [42] |
O.T. Majekodunmi, S. Kilic, and E. Ozdemir, Contributory roles of concentration and pH in CaCO3 growth inhibition for submicron particles synthesis with additive Ca2+, Powder Technol., 437(2024), art. No. 119588. |
| [43] |
T. Kawabata, Y. Takeda, M. Hori, K. Kandori, and T. Yaji, Partitioning of sodium into calcium carbonates synthesized at 10–40°C: Influence of organic ligands and temperature, Chem. Geol., 559(2021), art. No. 119904. |
| [44] |
|
| [45] |
Y.T. Gui, Z.M. Jiang, C.Y. Dai, and Q.B. Zhang, Enhanced effect of self-propagating subsequent heating on the expansive pressure on soundless chemical demolition agent, Constr. Build. Mater., 364(2023), art. No. 129866. |
| [46] |
Y.L. Wang, J. Yu, J.J. Wang, D. Xiang, H. Gu, and J.H. Cheng, Effects of sodium aluminate and quicklime on the properties of CSA grouting materials, J. Build. Eng., 58(2022), art. No. 105060. |
| [47] |
|
| [48] |
X.Y. Shen, P. Feng, Q. Zhang, et al., Toward the formation mechanism of synthetic calcium silicate hydrate (C–S–H)-pH and kinetic considerations, Cem. Concr. Res., 172(2023), art. No. 107248. |
The Author(s)
/
| 〈 |
|
〉 |