Effect of different drying methods on liquid penetration of Chinese fir plantation wood

L? Jianxiong, LIN Zhiyuan, JIANG Jiali, ZHAO Youke, JIANG Jinghui, GAO Ruiqing, YIN Yafang

PDF(335 KB)
PDF(335 KB)
Front. For. China ›› 2007, Vol. 2 ›› Issue (2) : 222-226. DOI: 10.1007/s11461-007-0036-x

Effect of different drying methods on liquid penetration of Chinese fir plantation wood

  • L? Jianxiong, LIN Zhiyuan, JIANG Jiali, ZHAO Youke, JIANG Jinghui, GAO Ruiqing, YIN Yafang
Author information +
History +

Abstract

Chinese fir plantation sapwood and heartwood boards were treated by three drying methods: radio frequency-vacuum drying (RFVD), conventional kiln drying (KD) and high temperature drying (HTD). The maximum amount of dyeing solution uptake by the capillary rising method was used to evaluate the liquid penetration of the treated wood. The pit aspiration ratio was determined by a semithin section method. Changes in wood microstructure were investigated using scanning electron microscopy. The results show that liquid penetration of Chinese fir sapwood after RFVD is significantly higher than that after KD and HTD. Liquid penetration of Chinese fir heartwood after RFVD is higher than that after HTD. Liquid penetration of Chinese fir sapwood is significantly higher than that of heartwood after three drying treatments. Low pit aspiration ratio and cracks of some bordered pits are the main reasons for the increase in liquid penetration after RFVD treatment.

Cite this article

Download citation ▾
L? Jianxiong, LIN Zhiyuan, JIANG Jiali, ZHAO Youke, JIANG Jinghui, GAO Ruiqing, YIN Yafang. Effect of different drying methods on liquid penetration of Chinese fir plantation wood. Front. For. China, 2007, 2(2): 222‒226 https://doi.org/10.1007/s11461-007-0036-x
PDF(335 KB)

Accesses

Citations

Detail

Sections
Recommended

/