Enhanced Electrochemical Performance and Theoretical Insights of Ni-Intercalated Ti3C2Tx MXene

Syed Muhammad Zain Mehdi , Hafiz Ghulam Abbas , Muzahir Ali , Syed Bilal Hasan Rizvi , Sung Ryul Choi , Jeung Choon Goak , Yongho Seo , Sunil Kumar , Naesung Lee

Energy & Environmental Materials ›› 2025, Vol. 8 ›› Issue (3) : e12876

PDF
Energy & Environmental Materials ›› 2025, Vol. 8 ›› Issue (3) : e12876 DOI: 10.1002/eem2.12876
RESEARCH ARTICLE

Enhanced Electrochemical Performance and Theoretical Insights of Ni-Intercalated Ti3C2Tx MXene

Author information +
History +
PDF

Abstract

Two-dimensional MXenes are renowned for their remarkable electrical conductivity and electrochemical activity making them highly promising for electrode applications. However, the restacking of MXene nanosheets impairs their functionality by reducing active sites and obstructing ionic transport. This study presents a facile synthesis approach for nickel-intercalated MXene, designed to enhance surface reactivity, avoid restacking, and achieve improved electrochemical performance. Electrochemical studies revealed that the nickel-MXene hybrid showed better cycling stability, retaining 83.7% of its capacity after 10 000 cycles and attaining an energy density of 26 Wh kg–1 at a power density of 1872 W kg–1. It also exhibited overpotentials of 109 and 482 mV at 10 and 100 mA cm–2, respectively, in the hydrogen evolution reaction. To predict the structural and electrical alterations caused by nickel inclusion, as well as to understand the intercalation mechanism, spin-polarized density functional theory calculations were carried out. The theoretical results showed an improved carrier concentration for nickel-MXene. Nickel-MXene possessed superior electronic characteristics and surplus active sites with hexagonal closed-packed (hcp) edge sites, which enhanced electrochemical properties. Our results demonstrate that nickel intercalation prevents the restacking of MXene but also significantly improves their electrochemical characteristics, making them ideal for energy storage and catalytic applications.

Keywords

DFT / HER / MXene / Ni intercalation / redox reaction

Cite this article

Download citation ▾
Syed Muhammad Zain Mehdi, Hafiz Ghulam Abbas, Muzahir Ali, Syed Bilal Hasan Rizvi, Sung Ryul Choi, Jeung Choon Goak, Yongho Seo, Sunil Kumar, Naesung Lee. Enhanced Electrochemical Performance and Theoretical Insights of Ni-Intercalated Ti3C2Tx MXene. Energy & Environmental Materials, 2025, 8(3): e12876 DOI:10.1002/eem2.12876

登录浏览全文

4963

注册一个新账户 忘记密码

References

[1]

S. Wee, X. Lian, E. Vorobyeva, A. Tayal, V. Roddatis, F. La Mattina, D. Gomez Vazquez, N. Shpigel, M. Salanne, M. R. Lukatskaya, ACS Nano 2024, 18, 10124.

[2]

M. R. Lukatskaya, O. Mashtalir, C. E. Ren, Y. Dall'Agnese, P. Rozier, P. L. Taberna, M. Naguib, P. Simon, M. W. Barsoum, Y. Gogotsi, Science 2013, 341, 1502.

[3]

J. L. Hart, K. Hantanasirisakul, A. C. Lang, B. Anasori, D. Pinto, Y. Pivak, J. T. van Omme, S. J. May, Y. Gogotsi, M. L. Taheri, Nat. Commun. 2019, 10, 522.

[4]

Y. Sun, J. Lee, N. H. Kwon, J. Lim, X. Jin, Y. Gogotsi, S.-J. Hwang, ACS Nano 2024, 18, 6243.

[5]

S. Li, Q. Shi, Y. Li, J. Yang, T. H. Chang, J. Jiang, P. Y. Chen, Adv. Funct. Mater. 2020, 30, 2003721.

[6]

M.-Q. Zhao, C. E. Ren, Z. Ling, M. R. Lukatskaya, C. Zhang, K. L. Van Aken, M. W. Barsoum, Y. Gogotsi, Adv. Mater. 2014, 27, 339.

[7]

M. Ghidiu, S. Kota, J. Halim, A. W. Sherwood, N. Nedfors, J. Rosen, V. N. Mochalin, M. W. Barsoum, Chem. Mater. 2017, 29, 1099.

[8]

K. Liang, R. A. Matsumoto, W. Zhao, N. C. Osti, I. Popov, B. P. Thapaliya, S. Fleischmann, S. Misra, K. Prenger, M. Tyagi, Adv. Funct. Mater. 2021, 31, 2104007.

[9]

M. D. Levi, M. R. Lukatskaya, S. Sigalov, M. Beidaghi, N. Shpigel, L. Daikhin, D. Aurbach, M. W. Barsoum, Y. Gogotsi, Adv. Energy Mater. 2015, 5, 1400815.

[10]

Y. Li, Y. Deng, J. Zhang, Y. Han, W. Zhang, X. Yang, X. Zhang, W. Jiang, Nanoscale 2019, 11, 21981.

[11]

C. Wang, S. Chen, H. Xie, S. Wei, C. Wu, L. Song, Adv. Energy Mater. 2019, 9, 1802977.

[12]

W. Xing, S. Qiao, X. Wu, X. Gao, J. Zhou, S. Zhuo, S. B. Hartono, D. Hulicova-Jurcakova, J. Power Sources 2011, 196, 4123.

[13]

B. K. Urhan, Ü. Demir, Electrochim. Acta 2019, 302, 109.

[14]

C. Ling, L. Shi, Y. Ouyang, Q. Chen, J. Wang, Adv. Sci. 2016, 3, 1600180.

[15]

X. Gao, X. Du, T. S. Mathis, M. Zhang, X. Wang, J. Shui, Y. Gogotsi, M. Xu, Nat. Commun. 2020, 11, 6160.

[16]

M. Hu, Z. Li, T. Hu, S. Zhu, C. Zhang, X. Wang, ACS Nano 2016, 10, 11344.

[17]

A. Sarycheva, Y. Gogotsi, Chem. Mater. 2020, 32, 3480.

[18]

H.-W. Wang, M. Naguib, K. Page, D. J. Wesolowski, Y. Gogotsi, Chem. Mater. 2016, 28, 349.

[19]

M. Hu, T. Hu, Z. Li, Y. Yang, R. Cheng, J. Yang, C. Cui, X. Wang, ACS Nano 2018, 12, 3578.

[20]

H. Zhou, S. Gu, Y. Lu, G. Zhang, B. Li, F. Dou, S. Cao, Q. Li, Y. Sun, M. Shakouri, Adv. Mater. 2024, 36, 2401856.

[21]

S. M. Z. Mehdi, M. Ali, M. F. Maqsood, N. Abbas, N. Lee, J. Alloys Compd. 2024, 988, 174250.

[22]

Y. Ding, Y. Chen, N. Xu, X. Lian, L. Li, Y. Hu, S. Peng, Nanomicro Lett 2020,

[23]

A. González-Elipe, G. Munuera, J. Espinos, J. Sanz, Surf. Sci. 1989, 220, 368.

[24]

V. Natu, M. Benchakar, C. Canaff, A. Habrioux, S. Celerier, M. W. Barsoum, Matter 2021, 4, 1224.

[25]

J. Li, X. Yuan, C. Lin, Y. Yang, L. Xu, X. Du, J. Xie, J. Lin, J. Sun, Adv. Energy Mater. 2017, 7, 1602725.

[26]

Z. U. Rehman, M. A. Raza, A. Tariq, U. N. Chishti, M. F. Maqsood, N. Lee, M. H. Awais, S. M. Z. Mehdi, A. Inam, J. Energy Storage 2020, 32, 101951.

[27]

H. Sun, Z. Ma, Y. Qiu, H. Liu, G. G. Gao, Small 2018, 14, 1800294.

[28]

S. Wu, K. Hui, K. Hui, K. H. Kim, J. Mater. Chem. A 2016, 4, 9113.

[29]

C. Choi, D. S. Ashby, D. M. Butts, R. H. DeBlock, Q. Wei, J. Lau, B. Dunn, Nat. Rev. Mater. 2020, 5, 5.

[30]

T. Liu, C. Jiang, B. Cheng, W. You, J. Yu, J. Power Sources 2017, 359, 371.

[31]

U. Latif, Z. U. Rehman, M. F. Maqsood, M. A. Raza, S. Ali, M. J. Iqbal, S. M. Z. Mehdi, N. Lee, J. Energy Stor. 2023, 73, 109024.

[32]

H. Zhou, Y. Lu, F. Wu, L. Fang, H. Luo, Y. Zhang, M. Zhou, J. Alloys Compd. 2019, 802, 259.

[33]

R. Ramachandran, C. Zhao, M. Rajkumar, K. Rajavel, P. Zhu, W. Xuan, Z.-X. Xu, F. Wang, Electrochim. Acta 2019, 322, 134771.

[34]

S. Kumar, S. M. Z. Mehdi, M. Ali, S. R. Choi, Y. Seojeong, M. Kim, M. Suleman, T. Singh, Y. Seo, J. Mater. Chem. 2024, C, 18732.

[35]

G. Kresse, J. Hafner, Phys. Rev. B 1993, 47, 558.

[36]

G. Kresse, J. Furthmüller, Phys. Rev. B 1996, 54, 11169.

[37]

J. P. Perdew, K. Burke, M. Ernzerhof, Phys. Rev. Lett. 1996, 77, 3865.

[38]

S. Grimme, S. Ehrlich, L. Goerigk, J. Comput. Chem. 2011, 32, 1456.

[39]

S. Grimme, J. Antony, S. Ehrlich, H. Krieg, J. Chem. Phys. 2010, 132, 154104.

RIGHTS & PERMISSIONS

2025 The Author(s). Energy & Environmental Materials published by John Wiley & Sons Australia, Ltd on behalf of Zhengzhou University.

AI Summary AI Mindmap
PDF

18

Accesses

0

Citation

Detail

Sections
Recommended

AI思维导图

/