Fused deposition modeling (FDM) fabricated polyethylene terephthalate glycol (PETG) may have a corrugated surface and voids between the layers, which can restrict performance in sliding contact. In this study, we investigated a low-cost surface engineering process where the tribologically challenging PETG substrate was structurally selected and the protective coating was the self-curing dental polymethyl methacrylate (PMMA). Three levels of each of the four FDM parameters were screened, with three independently printed specimens for each level of the parameter. Three-trial wear indices were analyzed using the original Taguchi smaller-the-better signal-to-noise (S/N) criterion, and factor-level means and sample standard deviations (SDs) were used to summarize the results for tensile strength, Rockwell R hardness (HRR), and inclined-plane static coefficient of friction (COF). The archived measurements were factor-level triplicates as opposed to responses associated with nine simultaneous L9 combinations. Selected PETG specimens were cross-hatched, acetone cleaned, dip-coated, and cured for 48 h. The coating was applied evenly at 0.5 mm on each face, increasing each reduced-section dimension by 1.0 mm in total. The coated condition had a mean maximum load 24.1% greater. Using condition-specific outer-section areas, the calculated tensile strength was 6.9% lower (27.15 ± 0.48 versus 25.29 ± 0.46 MPa), whereas the calculated tensile modulus was 13.8% higher (6.20 ± 0.25 versus 7.05 ± 0.19 MPa). Mean hardness was 44.2% higher (60.0 ± 0.8 versus 86.5 ± 0.7 HRR). The apparent PETG-equivalent wear index, calculated using a common PETG-density normalization due to the inability to separate the lost PMMA and PETG phases, was 50.0% lower ((27.77 ± 3.97) × 10-3 versus (13.88 ± 1.98) × 10-3 mm3 N-1 m-1). Static COF was 2.0% lower (0.1643 ± 0.0005 versus 0.1611 ± 0.0005), although the absolute change was small. The scanning electron microscopy (SEM) images revealed a more continuous coated surface and no large-scale delamination following the short duration abrasive test.
FDM / PETG / PMMA coating / tribology / abrasive wear / surface engineering / additive manufacturing
| [1] |
|
| [2] |
|
| [3] |
|
| [4] |
|
| [5] |
|
| [6] |
|
| [7] |
|
| [8] |
|
| [9] |
|
| [10] |
|
| [11] |
|
| [12] |
|
| [13] |
|
| [14] |
|
| [15] |
|
| [16] |
|
| [17] |
|
| [18] |
|
| [19] |
|
| [20] |
|
| [21] |
|
| [22] |
|
| [23] |
|
| [24] |
|
| [25] |
|
| [26] |
|
| [27] |
|
| [28] |
|
| [29] |
|
| [30] |
|
| [31] |
|
| [32] |
|
| [33] |
|
| [34] |
|
| [35] |
|
| [36] |
|
| [37] |
|
| [38] |
ASTM International (2014) Standard test method for tensile properties of plastics. ASTM D638-14. West Conshohocken, PA. https://store.astm.org/d0638-14.html |
| [39] |
ASTM International (2023) Standard test method for Rockwell hardness of plastics and electrical insulating materials. ASTM D785-23. West Conshohocken, PA. https://store.astm.org/d0785-23.html |
| [40] |
ASTM International (2005) Standard test method for wear testing with a pin-on-disk apparatus. ASTM G99-05. West Conshohocken, PA. https://store.astm.org/g0099-05.html |
| [41] |
ASTM International (2024) Standard guide for determination of static coefficient of friction of test couples using an inclined plane testing device. ASTM G219-24. West Conshohocken, PA. https://store.astm.org/g0219-24.html |
| [42] |
|
/
| 〈 |
|
〉 |