Abstract

The solid fast ionic conductor was synthesized by the sol-gel-hydrothermal method. The influences of dispersion reagent, the alkalinity and the calcination temperature on the surface morphology of nanopowders, the electric conductivity were discussed. When PEG 12000 was used as the dispersion reagent, the alkalinity was 1.0% and the calcination temperature was 550ºC; the electric conductivity at ambience temperature of the inorganic nanopowder of lithium fast ionic conductor synthesized was 2.59 ? 10-3 S•cm-1.

Keywords

lithium fast ionic conductor, inorganic nanopowder, sol-gel-hydrothermal method

Cite this article

Download citation ▾
null. Preparation of lithium fast ionic conductor by sol-gel-hydrothermal method. Front. Chem. China, 2006, 1(4): 374-377 DOI:10.1007/s11458-006-0047-4

登录浏览全文

4963

注册一个新账户 忘记密码

References

AI Summary AI Mindmap
PDF (804KB)

575

Accesses

0

Citation

Detail

Sections
Recommended

AI思维导图

/